Bayani: SC810 UHT POLYMER RETARDER
Bayanin Samfura
1.SC810 ne mai matsananci-high zafin jiki polymer retarder, wanda ke taimaka tsawanta lokacin thickening na siminti slurry domin ya ci gaba da pumpable, da kuma tabbatar da isasshen famfo lokaci ga wani hadari.
aikin siminti.
2.Thickening lokacin yana da alaƙa mai layi tare da sashi da zafin jiki. Za a iya cimma madaidaicin kusurwa mai kauri.
3.Karfin simintin saiti yana haɓaka da sauri.
4.Yi amfani da ƙasa 204.4℃ (400℉, BHCT).
5.Has mai kyau jituwa tare da polymer ruwa asarar ƙari, kuma kadan tasiri a kan high zafin jiki ruwa asarar yi.
6.SC810 jerin kunshi L-type ruwa, LA irin anti-daskarewa ruwa, PP irin high tsarki foda, PD irin bushe-mixed foda da PT irin dual-amfani foda.
Ƙayyadaddun bayanai
Nau'in | Bayyanar | Yawan yawa, g/cm3 | Ruwa-Rauni |
Saukewa: SC810L (nau'in misali) | Fari ko ratsi ruwan rawaya | 1.10± 0.05 | Mai narkewa |
Saukewa: SC810L-A (nau'in daskarewa) | Fari ko ratsi ruwan rawaya | 1.15± 0.05 | Mai narkewa |
Nau'in | Bayyanar | Yawan yawa, g/cm3 | Ruwa-Rauni |
Saukewa: SC810P-P | Farar fari ko ratsi rawaya foda | 0.80± 0.20 | Mai narkewa |
Saukewa: SC810P-D | Grey foda | 1.00± 0.10 | Rarrabe mai narkewa |
Saukewa: SC810P-T | Farar fari ko ratsi rawaya foda | 1.00± 0.10 | Mai narkewa |
Shawarwari sashi
Nau'in | SC810L (-A) | Saukewa: SC810P-P | Saukewa: SC810P-D | Saukewa: SC810P-T |
Matsakaicin Sashi (BWOC) | 2.0-8.0% | 0.5-2.5% | 1.5-4.0% | 1.5-4.0% |
Ayyukan Siminti Slurry
Abu | Yanayin gwaji | Nunin Fasaha |
Daidaituwar farko, Bc | 180 ℃/73 min, 115mPa | ≤30 |
40-100BC lokacin kauri, min | ≤40 | |
Daidaitaccen lokacin kauri | daidaitacce | |
Ƙimar canji kwatsam na daidaito, Bc | ≤10 | |
Ruwa kyauta,% | ≤1.4 | |
Ƙarfin ƙarfi don 24h, mPa | 180 ℃, 20.7mPa | ≥14 |
Abun da ke ciki: API Class G (HSR) 600g, gari na silica 210g (35%), silica fume 36g (6%), ruwa mai gauraya 342g (ciki har da additives na ruwa), defoamer 1.8g (0.3%), SC810. | ||
Note: The sashi na SC810 ne m karkashin te precondition na daidaitawa lokacin thickening kewayon siminti slurry a 180 ℃ zuwa 230-420 min. |
Daidaitaccen Marufi da Ma'aji
1.Ya kamata a yi amfani da samfuran nau'in ruwa a cikin watanni 12 bayan samarwa. Kunshe a cikin ganga filastik 25kg, 200L da galan 5 US. Ya kamata a yi amfani da samfuran foda na nau'in PP/D a cikin 24
watanni da PT nau'in samfurin foda ya kamata a yi amfani da su a cikin watanni 18 bayan samarwa. Kunshe a cikin jaka 25kg.
2.Customized kunshe-kunshe kuma akwai. Da zarar ya ƙare, za a gwada kafin amfani.
Kunshin
25KG/BAG ko kamar yadda kuka nema.
Adana
Ajiye a wuri mai busasshiyar iska.
Matsayin Gudanarwa
Matsayin Duniya.